Showerthought: a hand block beats a DA every time on long panels
I know everybody loves their DA and I use mine plenty, but for big flat stuff like a truck bedside or a door skin, hand blocking with a long board wins for me and it's not close. Last month I did a bedside on a Silverado and started with the DA on 180 like usual, and I could feel it digging low spots it wasn't supposed to touch. Switched to a 16 inch block and wet paper and the panel told me the truth within about 10 minutes, high spots and all. Yeah my arm was cooked by the end of the day, but the primer laid out flat and I only had one small spot to touch up before sealer. The DA is fast, sure, but fast got me chasing waves I made myself. Maybe it's just me but I think guys lean on the DA because it feels like progress, not because the panel is actually getting straighter. What grit are you all running on your long boards for a first cut?